Sublimation Time and Temperature Chart

Flat heat press and mug press on a workbench with a wrapped mug and a white t-shirt

Most sublimation blanks press at 180°C. What changes from one blank to the next is the time and the pressure: a polyester t-shirt needs 120 seconds at normal pressure, an 11oz mug needs 180 seconds at medium pressure, and a photo slate needs 300 to 360 seconds at light pressure. The chart below lists the recommended settings for every blank we sell that has published press settings, grouped by product type.

Use these settings as your starting point, then run a test piece on your own press before a full batch. Presses vary, and the sections after the chart explain what to change if a result looks faded, scorched or blurred.

Sublimation temperature and time chart

Times are in seconds. Pressure is given as it appears on each product page. Where several products share the same settings, they are listed together.

Mugs

Blank Temperature Time Pressure
11oz Orca Mugs, AAA Grade (white) 180°C 180s Medium
11oz Inner and Handle Coloured Mugs (pink, light blue, navy blue, black, grey, baby blue, green, red, maroon, purple, orange, yellow) 180°C 180s Medium
11oz Polymer Unbreakable Mug 160°C 120s Medium

Tumblers and water bottles

Blank Temperature Time Pressure
20oz Tumbler (600ml) 180°C 30s Medium
20oz Tumbler With Handle 180°C 30s Medium
40oz Tumbler (white) 180°C 160s Medium
Stainless Steel Water Bottles (pink, blue, yellow, double insulated white) 180°C 30s High
Explorer Water Bottles, 600ml (black, blue) 180°C 60s Medium

Christmas blanks

Blank Temperature Time Pressure
Christmas Baubles, 8cm (red, silver) 180°C 60s Medium
Ceramic Ornaments, 3" with gold string (round, star, heart) 190°C 120s Medium
Christmas Stockings (small kids, large, luxury 290gsm) 190°C 50 to 60s Medium to firm
Linen Santa Sack, large (50 x 68cm) 185°C 60s Medium

Clothing and textiles

Blank Temperature Time Pressure
100% Polyester T-Shirts, adult and kids (white, grey) 180°C 120s Normal
100% Polyester Hoodies, adult and kids (white, grey) 180°C 120s Normal
100% Polyester Crop Top, adult (white) 180°C 120s Normal
Polyester Aprons (adult, kids) 180°C 120s Medium
Soft Polyester Tote Bags (white or natural, large or small) 180°C 60s Medium

Bags, cases and tech accessories

Blank Temperature Time Pressure
Leather Flip Phone Cases (all iPhone and Galaxy models) 180°C 80s Normal
iPad Cases (iPad Pro 9.7", iPad Pro 12.9", iPad Mini 4) 180°C 80s Medium
Phone Stand (black) 180°C 80s Medium
Neoprene Laptop Sleeves (16 inch, 18 inch) 180°C 200s High
Large Sublimation Backpack 180°C 200s High
Pencil Case (black) 180°C 120s Medium
Lunch Bag (black) 180°C 120s Medium
Passport Holder (white) 180°C 60s Medium
Spiral Notepads with plastic cover (A4, A5, A6) 180°C 60s Medium

Jewellery and keyrings

Blank Temperature Time Pressure
Oblong Metal Keyrings (silver, rose gold, gold) 180°C 80s Medium
Rectangle Keyring, double sided 180°C 80s Medium
Circle Necklace and Heart Necklace 180°C 80s Medium

Hard blanks: coasters, slate, crystal and glass

Blank Temperature Time Pressure
Unisub Square Hardboard Coaster, 9 x 9cm raw back 180°C 110s Medium
MDF Cork Back Coaster 180°C 80s Medium
Crystal Blocks (small 8 x 6 x 1.5cm, large 15 x 20 x 1.9cm) 180°C 160s Medium
Square Photo Rock Slate Coaster, matte 180°C 360s Light
Square Photo Rock Slate Coaster, gloss 180°C 300s Light
Photo Rock Slate, 15 x 20cm rectangle, glossy 180°C 360s Light, face down
Photo Rock Slate, 20 x 20cm square, glossy 180°C 300s Light
Glass Cutting Boards (large and small chinchilla, large and small smooth, 12" round smooth) 180°C 180s Medium

You can browse each group in our sublimation mugs, Christmas, sublimation clothing and other sublimation blanks collections. Each product page shows the same settings.

If the print looks faded

A pale or washed-out print usually means not enough ink has turned to gas and moved into the blank. Check these in order:

  • Time. Add 10 to 15 seconds and press a test piece. This is the smallest change and the easiest to reverse.
  • Pressure. On a flat press, light pressure can leave pale patches where the paper did not touch the surface. Increase it one step.
  • Actual temperature. A press that shows 180°C may be running cooler. Check the platen with an infrared thermometer.
  • The print itself. Sublimation ink looks dull on paper before pressing, which is normal. If the pressed result is still pale, check that you printed on the coated side of the paper at high quality.

Our guide to prints coming out too dark or too light covers the printer-side causes in more detail.

If the print looks scorched or yellowed

Brown or yellow tinting on white areas, or a shiny square mark on fabric, points to too much heat or too much time. Reduce the time first, by 10 to 15 seconds, before you lower the temperature. On garments, a square outline around the design is usually a press mark from the platen edge rather than scorching; our guide on avoiding press marks on fabric explains how to prevent it. Hoodies and other thick items are more prone to marks because of seams, zips and pockets under the platen.

If the print looks ghosted or blurred

Ghosting is a faint second image offset from the main one. It happens when the paper moves during pressing or as the press opens, and the hot ink transfers a second time. Fix it by holding the paper in place with high temperature heat tape on every edge, and by lifting the paper off in one clean movement once the press opens. On mugs and tumblers, wrap the paper tightly so there are no gaps between the paper and the surface. See our guide to using heat-resistant tape for placement tips.

Allowing for differences between presses

The settings in the chart are a starting point, not a guarantee, because no two presses heat in exactly the same way. Things to check on your own press:

Mug wrapped in sublimation paper and heat-resistant tape inside a mug press

  • Display versus platen temperature. Measure the platen surface with an infrared thermometer after preheating. If it reads 5 to 10 degrees off the display, adjust your set temperature to compensate.
  • Even heating. Measure the centre and each corner. Cooler corners show up as faded edges on large prints. Our guide on heat presses that are not heating evenly covers this.
  • Pressure scale. Light, medium and high are relative. On a manual clamshell press, medium pressure usually means the handle closes with firm effort but no strain.
  • Mug and tumbler presses. Element size and fit vary, so a tumbler that sits loosely in the element will need longer than one held tightly.

Write down the settings that work for each blank on your press, and use them every time. Our guide to heat press machines for sublimation compares the main types.

Polyester fabric versus coated hard blanks

Sublimation ink bonds with polyester. On fabric, the polyester is the fibre itself, which is why our t-shirts, hoodies, aprons and tote bags are 100% polyester and press at 180°C for 60 to 120 seconds. Cotton has no polyester to bond with, so the ink washes out.

Sublimation paper placed on a white polyester t-shirt in a heat press

Hard blanks such as mugs, slate, crystal, glass, metal keyrings and coasters are made from materials that cannot take sublimation ink on their own. They carry a polyester-based coating on the print surface, and that coating is what receives the ink. Coated blanks usually need more time than fabric, because the heat has to pass through a solid material that soaks up heat, such as ceramic, stone or glass. That is why photo slate needs 300 to 360 seconds and crystal blocks 160 seconds, while a t-shirt needs 120.

Two practical points follow from this. Coated surfaces can scratch, so handle them by the edges and keep them clean before pressing. Hard blanks also stay hot for a long time after pressing, so use heat-resistant gloves and let them cool on a heat-safe surface.

FAQs

What temperature should I use for sublimation mugs?

Our 11oz white Orca mugs and 11oz inner and handle coloured mugs are pressed at 180°C for 180 seconds at medium pressure. The 11oz Polymer Unbreakable Mug is different: it is pressed at 160°C for 120 seconds at medium pressure.

Is 200°C too hot for sublimation?

For the blanks in this chart, yes. The highest setting we list is 190°C, for ceramic ornaments and Christmas stockings. Pressing hotter than the recommended temperature increases the risk of scorching and yellowing, especially on white areas.

Should I change the time or the temperature first?

Change the time first, in steps of 10 to 15 seconds. Temperature changes have a bigger effect and are harder to judge. Only adjust the temperature once you have confirmed with a thermometer that your press is reading accurately.

Why does my print look dull before pressing?

Sublimation ink always looks muted on paper. The full colour only appears once the ink is heated and moves into the polyester or coating. Judge colour on the pressed item, not on the printed sheet.

Why do Christmas stockings have a time range instead of a single time?

The stockings are listed at 190°C for 50 to 60 seconds at medium to firm pressure. Start at 50 seconds on a test piece and move towards 60 if the print looks pale.